Hastelloy X Barni issiqlik bilan ishlov berish jarayoni

 

Plastinka qattiq eritmasi bilan ishlov berish: 1150 daraja ± 10 daraja, 2-15min, tez havo sovutish.

Payvandlash qismlari yoki olov silindrli ishlov berish: 980 daraja ± 10 daraja, 60 min, havo sovutish.

Ishlov berishdan keyin stressni engillashtiradigan ishlov berish: 870 daraja ±10 daraja, 30-60min, havo sovutish.

Qismlarning barqaror o'lchamlari bilan ishlov berish: 760 daraja ± 10 daraja, 2 soat, havo sovutish.